Comprehensive reference on state-of-the-art aerospace materials, reviewing the latest developments in the field and providing guidance on machining challenges
Grinding of Single-Crystal Superalloys provides a comprehensive understanding of grinding technology for single-crystal nickel-based superalloys. It explores and analyzes grinding mechanisms and characteristics using both theoretical and simulation approaches. Grinding behavior in conventional and micro grinding processes are evaluated and compared.
The book assesses the surface integrity of single-crystal nickel-based superalloys under different grinding conditions. Simulation and theoretical models for predicting temperature and residual stresses in profile grinding, facilitating optimization, and control are summarized and validated.
Grinding of Single-Crystal Superalloys discusses sample topics including:
Grinding of Single-Crystal Superalloys is an essential reference for industry professionals and researchers seeking to understand the machining theory and practice of this important type of material, especially in the field of aerospace components manufacturing.
Author: Wenfeng Ding
ISBN-10: 3527355227
ISBN-13: 9783527355228
Publisher: Wiley-Vch
Language: English
Published: 01/21/2026
Pages: 288
Format: Hardcover
Weight: 1.40lbs
Size: 9.61h x 6.69w x 0.63d
Prof. Wenfeng Ding dedicated his research in the field of advanced manufacturing theory and technologies.
Dr. Qing Miao dedicated his research in the field of advanced material microstructure characterization and high-quality and high-efficiency grinding technology of nickel-based superalloys.
Dr. Yao Sun researches basic theory and technology of the grinding process of difficult-to-machine materials, intelligent manufacturing, and micro-scale machining.
Ning Qian is an Associate Professor at Nanjing University of Aeronautics and Astronautics (NUAA).
Biao Zhao is an Associate Professor of Mechanical Engineering and Master's Tutor at Nanjing University of Aeronautics and Astronautics, China.
Prof. Jiuhua Xu teaches and researches the grinding of difficult-to-cut materials.